Injection Molding Tolerances: Chart, Standards and How to Specify Them
Table of Contents
Need expert machining solutions? Our team at Tuowei Precision is here to assist with all your manufacturing needs. Get in touch today for a quote on your ongoing or upcoming projects!
A typical injection molding tolerance is about ±0.1 mm on a small dimension, and about ±0.05 mm when the part, material and mold are all designed for precision. Molded plastic cannot match machined metal, because the part shrinks as it cools and the amount of shrink varies. This guide gives a tolerance chart by material, explains what controls tolerance and shows how to specify it without overpaying.
What are injection molding tolerances?
A tolerance is the allowed variation on a dimension. In injection molding there are two separate tolerances, and mixing them up causes most quoting disputes.
- Mold (tooling) tolerance: how accurately the steel cavity is machined. This is tight, because the mold is CNC machined and EDM cut.
- Part tolerance: how much the molded parts vary from shot to shot and from the nominal dimension. This is always looser, because it adds shrinkage, process variation and warp on top of the mold tolerance.
Your drawing specifies part tolerance. The molder then builds the mold tighter than that to leave room for process variation.
Injection molding tolerance chart by material
The values below are typical industry guidance for a dimension of about 25 mm, molded in a well-built steel tool. Larger dimensions need more allowance. Always confirm achievable values with your molder for your specific part.
| Material | Type | Typical shrinkage | Commercial tolerance | Fine tolerance |
|---|---|---|---|---|
| ABS | Amorphous | 0.4–0.7% | ±0.10 mm | ±0.05 mm |
| PC (polycarbonate) | Amorphous | 0.5–0.7% | ±0.10 mm | ±0.05 mm |
| PMMA (acrylic) | Amorphous | 0.2–0.8% | ±0.10 mm | ±0.05 mm |
| PA6 / PA66 (nylon) | Semi-crystalline | 0.7–2.0% | ±0.15 mm | ±0.08 mm |
| POM (acetal) | Semi-crystalline | 1.8–2.5% | ±0.15 mm | ±0.08 mm |
| PP (polypropylene) | Semi-crystalline | 1.0–2.5% | ±0.20 mm | ±0.10 mm |
| PEEK | Semi-crystalline | 1.0–1.5% | ±0.13 mm | ±0.05 mm |
The pattern to remember: amorphous plastics shrink less and more evenly, so they hold tighter tolerances. Semi-crystalline plastics shrink more and differently along and across the flow, so they need more allowance. Glass-filled grades shrink less overall but can warp more.

What controls the tolerance you can achieve
- Material shrinkage. Higher and less uniform shrinkage means wider variation. This is the biggest single factor.
- Part size. Variation scales with length. A 200 mm dimension cannot hold the same tolerance as a 20 mm one.
- Wall thickness. Uniform walls cool evenly. Thick sections sink and thin-to-thick transitions warp.
- Part geometry. Long flat panels, unsupported walls and asymmetric shapes warp. Ribs and gussets help.
- Mold design and quality. Gate location, cooling layout and steel quality decide how evenly the part fills and cools.
- Features across the parting line. Dimensions formed by both mold halves, or by slides, carry extra variation from mold alignment.
- Process control. Melt temperature, pressure, hold time and cooling time must stay stable shot after shot.
- Conditions after molding. Nylon absorbs moisture and grows. Measure parts at a stated temperature and conditioning state.
Tolerance standards: ISO 20457 vs ISO 2768
- ISO 20457 is the current international standard for tolerances of plastic molded parts. It replaced the widely used German standard DIN 16742. It groups parts into tolerance classes based on material, process and dimension size.
- ISO 2768 gives general tolerances for machined parts. It is often copied onto plastic part drawings by habit, but it was not written for molded plastics and frequently demands more than molding can deliver at a sensible cost.
- SPI/PLASTICS guidelines are common on North American drawings. They list commercial and fine tolerances by material.
If your title block defaults to ISO 2768, change it for molded parts. Reference ISO 20457 or state explicit tolerances on critical features instead.
What tight tolerances cost
Tightening a tolerance does not just add inspection. It changes the project.
- The mold needs higher-grade steel, more precise machining and often extra cooling circuits.
- More mold trials are needed to tune dimensions (“steel-safe” adjustments after first samples).
- Cycle times get longer to stabilize cooling.
- Scrap rate rises, and more parts must be measured.
Moving one critical feature from commercial to fine tolerance is usually manageable. Applying fine tolerance to every dimension can multiply tooling cost and lead time for no functional gain.

How to specify tolerances on a molded part drawing
- Identify the features that actually control fit or function. Most parts have fewer than ten.
- Put explicit tolerances on those features only.
- Apply a general molding tolerance to everything else.
- Keep critical dimensions within one mold half where possible, away from the parting line and slides.
- State the material grade, since tolerance depends on it.
- Define measurement conditions: temperature, time after molding and conditioning for nylon.
- Ask for a first-article inspection report on the critical features.
Design tips that help parts hold tolerance
- Keep wall thickness uniform, and core out thick sections.
- Add draft so parts release without distortion.
- Use ribs for stiffness instead of thicker walls.
- Use generous radii at corners to reduce stress and warp.
- Choose an amorphous material when tight tolerance matters more than chemical resistance.
- If one feature needs machining-level accuracy, mold the part and machine that feature afterward, or use an insert.
Injection molding vs CNC machining tolerances
| Injection molding | CNC machining | |
|---|---|---|
| Typical tolerance | ±0.1 mm | ±0.05 mm or better |
| Best case | about ±0.05 mm | down to ±0.005 mm |
| Main limit | Shrinkage and warp | Machine and tool accuracy |
| Cost of tightening | Tooling changes and trials | Extra machining and inspection time |
For low volumes with very tight tolerances, machining the plastic part is often the better route. For high volumes, design the part so molding tolerances are enough.
Tight-tolerance injection molding: when it is worth it
Tight-tolerance injection molding means holding roughly ±0.05 mm or better on critical dimensions. It is achievable, but only when the whole project is built around it.
- Material: a low-shrink amorphous or glass-filled grade with good dimensional stability.
- Part design: uniform wall thickness, adequate draft angles and critical dimensions kept in one mold half.
- Tool design: hardened steel, precise cavity machining, balanced filling and cooling close to the cavity.
- Process: controlled mold temperature, pressure and cycle time, monitored during production.
- Measurement: an agreed method, fixture and conditioning time.
Use it for snap fits, sealing faces, bearing bores, gear features and parts that fit together with machined or metal components. Do not use it for cosmetic surfaces or free dimensions.
Tolerances by feature type
Dimensional tolerance is only one kind. A molded part drawing usually controls several feature types, and each behaves differently.
| Feature | What affects it most | Design advice |
|---|---|---|
| Linear dimensions | Shrinkage, size of the dimension | Tolerance grows with length; keep critical ones short |
| Hole diameter | Core pin size, shrink toward the pin | Holds well; specify the functional fit |
| Hole depth | Core pin deflection, shrink | Blind holes deeper than about 3× diameter are harder to hold |
| Wall thickness | Flow, cooling, mold alignment | Keep uniform; avoid thick-to-thin steps |
| Flatness and straightness | Warp from uneven cooling | Add ribs; avoid large unsupported flat areas |
| Position of features | Mold alignment, shrink between features | Dimension from one datum in the same mold half |
| Draft angles | Needed for ejection | Allow 1–2° per side, and state whether dimensions apply at the wide or narrow end |
Tolerance stack-up in assemblies
When several molded parts fit together, their tolerances add up. Three parts at ±0.1 mm each can be 0.3 mm out in the worst case. Work out the stack-up before you fix individual tolerances, and loosen everything that does not affect the fit. This is where most unnecessary tight tolerances come from.
Mold flow analysis, T1 samples and steel-safe tuning
Three steps bring a molded part into tolerance.
- Mold flow analysis simulates filling, cooling and warp before steel is cut. It predicts shrink differences along and across the melt flow direction and guides gate and cooling design.
- T1 samples are the first shots from the finished tool. They are measured against the drawing to see where the real part lands.
- Steel-safe tuning adjusts the mold. Cavities are cut slightly undersize on critical features, so steel can be removed to move a dimension into tolerance.
Agree in advance how many sampling rounds are included and which dimensions will be reported.
How the standards relate: DIN 16901, DIN 16742 and ISO 20457
Older drawings often cite DIN 16901. It was replaced by DIN 16742, which in turn became the basis of ISO 20457. All three sort parts into tolerance groups by material shrinkage and manufacturing effort, then give allowable deviations by nominal dimension range. If your drawing still cites DIN 16901, updating it to ISO 20457 avoids confusion with newer suppliers.
Material selection and part tolerances
Material selection is the first tolerance decision you make. Different materials shrink by different amounts, so the same mold steel gives different part tolerances in ABS and in polypropylene. For injection molded parts that must fit an assembly, choose the resin with the tolerance in mind, not only its strength or price.
Some applications need more than the material can give. When dimensional tolerances on one feature are tighter than the tolerance range of the resin, the usual engineering answers are to redesign the joint, add an insert, or machine that feature after molding. Discuss these options during part design, before the production process is fixed, because changing a mold later is expensive. It is important to write the agreed specifications on the drawing so the molder and the buyer measure the injection molded part the same way.
About The Author
Andy
Manufacturing Engineer at tuoweiprecision
Written by Andy, Manufacturing Engineer at TUOWEI Precision. Andy specializes in CNC machining, precision manufacturing, and production engineering, with hands-on experience supporting projects from rapid prototyping through full-scale production. He works closely with engineering and manufacturing teams to evaluate materials, tolerances, machining processes, and design manufacturability. His articles provide practical, technically informed insights to help engineers and buyers make better manufacturing decisions, optimize production efficiency, and achieve consistent part quality. Explore TUOWEI Precision’s CNC machining and custom manufacturing solutions for your next project.
Partner with Tuowei Precision to Shape Your Vision
From rapid prototypes to scalable production, Tuowei Precision delivers reliable CNC machining with accuracy and consistency at every step. Start your project today.
- Established engineering skills.
- Global project support
- Advanced CNC solutions
- Co-creation of products.
- Expandable capacity of production.
- All uploads are secure and confidential
Explore Insights & Innovation
Read our latest guides on CNC machining, materials, finishing and industry trends to make better production decisions.