| Property | Value |
|---|---|
| Mechanical Properties | |
| Ultimate tensile strength | 330 – 350 MPa |
| Yield strength | 140 – 150 MPa |
| Elongation at break | 20 – 23 % |
| Physical Properties | |
| Corrosion resistance | Moderate |
| Magnetism | Non-magnetic |
| Weldability | High |
| Post Treatments | |
| Post-Processing | Annealing |