{"id":649,"date":"2025-01-25T11:14:26","date_gmt":"2025-01-25T11:14:26","guid":{"rendered":"https:\/\/tuoweiprecision.com\/?post_type=material&#038;p=649"},"modified":"2025-04-28T18:37:29","modified_gmt":"2025-04-28T18:37:29","slug":"tool-steel-s7-1-2355-50crmov13-15-annealed-state","status":"publish","type":"material","link":"https:\/\/tuoweiprecision.com\/fr\/materiel\/tool-steel-s7-1-2355-50crmov13-15-annealed-state\/","title":{"rendered":"Tool steel S7 | 1.2355 | 50CrMoV13-15 \u2013 Annealed state"},"content":{"rendered":"<!DOCTYPE html>\n<html lang=\"en\">\n<head>\n    <meta charset=\"UTF-8\">\n    <meta name=\"viewport\" content=\"width=device-width, initial-scale=1.0\">\n    <style>\n        table {\n            width: 100%;\n            border-collapse: collapse;\n            font-size: 14px; \/* Default WordPress font size *\/\n        }\n        th, td {\n            border: 1px solid black;\n            padding: 8px;\n            text-align: left;\n        }\n        th {\n            font-weight: bold;\n        }\n        td:first-child {\n            width: 50%;\n        }\n        td:last-child {\n            width: 50%;\n        }\n    <\/style>\n<\/head>\n<body>\n\n<table>\n    <thead>\n        <tr>\n            <th>Propri\u00e9t\u00e9<\/th>\n            <th>Valeur<\/th>\n        <\/tr>\n    <\/thead>\n    <tbody>\n        <tr>\n            <td colspan=\"2\"><strong>Propri\u00e9t\u00e9s m\u00e9caniques<\/strong><\/td>\n        <\/tr>\n        <tr>\n            <td>R\u00e9sistance ultime \u00e0 la traction<\/td>\n            <td>640 &#8211; 670 MPa<\/td>\n        <\/tr>\n        <tr>\n            <td>Limite d'\u00e9lasticit\u00e9<\/td>\n            <td>370 &#8211; 380 MPa<\/td>\n        <\/tr>\n        <tr>\n            <td>Module de Young (module d'\u00e9lasticit\u00e9)<\/td>\n            <td>190 GPa<\/td>\n        <\/tr>\n        <tr>\n            <td>Allongement \u00e0 la rupture<\/td>\n            <td>21 &#8211; 25 %<\/td>\n        <\/tr>\n\n        <tr>\n            <td colspan=\"2\"><strong>Propri\u00e9t\u00e9s physiques<\/strong><\/td>\n        <\/tr>\n        <tr>\n            <td>Magn\u00e9tisme<\/td>\n            <td>Magn\u00e9tique<\/td>\n        <\/tr>\n        <tr>\n            <td>Soudabilit\u00e9<\/td>\n            <td>Pauvre<\/td>\n        <\/tr>\n\n        <tr>\n            <td colspan=\"2\"><strong>Propri\u00e9t\u00e9s thermiques<\/strong><\/td>\n        <\/tr>\n        <tr>\n            <td>Temp\u00e9rature de service maximale<\/td>\n            <td>165 &#8211; 215 \u00b0C<\/td>\n        <\/tr>\n        <tr>\n            <td>Coefficient de dilatation thermique<\/td>\n            <td>10.7 &#8211; 11.2 \u00d7 10<sup>-6<\/sup>\/\u00baC<\/td>\n        <\/tr>\n        <tr>\n            <td>Conductivit\u00e9 thermique<\/td>\n            <td>42.3 &#8211; 45.7 W\/(m\u22c5\u00b0C)<\/td>\n        <\/tr>\n\n        <tr>\n            <td colspan=\"2\"><strong>Propri\u00e9t\u00e9s \u00e9lectriques<\/strong><\/td>\n        <\/tr>\n        <tr>\n            <td>R\u00e9sistivit\u00e9 \u00e9lectrique<\/td>\n            <td>24.5 &#8211; 30.2 \u03bc\u03a9*cm<\/td>\n        <\/tr>\n\n        <tr>\n            <td colspan=\"2\"><strong>Post-traitements<\/strong><\/td>\n        <\/tr>\n        <tr>\n            <td>Post-traitement<\/td>\n            <td>Durcissement et recuit<\/td>\n        <\/tr>\n        <tr>\n            <td>Compatibilit\u00e9 avec l'anodisation<\/td>\n            <td>Ne convient pas<\/td>\n        <\/tr>\n\n        <tr>\n            <td colspan=\"2\"><strong>Applications courantes<\/strong><\/td>\n        <\/tr>\n        <tr>\n            <td>Cutting tools<\/td>\n            <td>Hot forging &#038; extrusion tools<\/td>\n        <\/tr>\n        <tr>\n            <td>Matrices de formage \u00e0 froid<\/td>\n            <td>Shearing tools<\/td>\n        <\/tr>\n    <\/tbody>\n<\/table>\n\n<\/body>\n<\/html>","protected":false},"excerpt":{"rendered":"<p>Property Value Mechanical Properties Ultimate tensile strength 640 &#8211; 670 MPa Yield strength 370 &#8211; 380 MPa Young&#8217;s modulus (modulus of elasticity) 190 GPa Elongation at break 21 &#8211; 25 % Physical Properties Magnetism Magnetic Weldability Poor Thermal Properties Maximum service temperature 165 &#8211; 215 \u00b0C Thermal expansion coefficient 10.7 &#8211; 11.2 \u00d7 10-6\/\u00baC Thermal [&hellip;]<\/p>","protected":false},"featured_media":0,"parent":0,"template":"","format":"standard","meta":{"_acf_changed":false,"_seopress_robots_primary_cat":"","_seopress_titles_title":"","_seopress_titles_desc":"","_seopress_robots_index":"","footnotes":""},"material-category":[15,34],"class_list":["post-649","material","type-material","status-publish","format-standard","hentry","material-category-cnc-machining-metals","material-category-tool-steel"],"acf":[],"_links":{"self":[{"href":"https:\/\/tuoweiprecision.com\/fr\/wp-json\/wp\/v2\/material\/649","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/tuoweiprecision.com\/fr\/wp-json\/wp\/v2\/material"}],"about":[{"href":"https:\/\/tuoweiprecision.com\/fr\/wp-json\/wp\/v2\/types\/material"}],"version-history":[{"count":0,"href":"https:\/\/tuoweiprecision.com\/fr\/wp-json\/wp\/v2\/material\/649\/revisions"}],"wp:attachment":[{"href":"https:\/\/tuoweiprecision.com\/fr\/wp-json\/wp\/v2\/media?parent=649"}],"wp:term":[{"taxonomy":"material-category","embeddable":true,"href":"https:\/\/tuoweiprecision.com\/fr\/wp-json\/wp\/v2\/material-category?post=649"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}